Researchers in China have identified why repeated screen printing of photoresist can erode the performance of copper-plated silicon heterojunction (HJT) solar cells, and have proposed a modified screen design that limits the damage. The work targets a step that is central to copper metallization, an approach pursued as a way to cut silver consumption and metallization cost in high-efficiency cells.
Screen printing is a workhorse metallization technique in solar cell manufacturing, but its mechanical pressure and thermal treatments can harm the sensitive passivating contact structures of HJT devices, raising recombination losses and lowering conversion efficiency. Because copper plating relies on a screen-printed photoresist pattern, the reliability of that printing step matters for the plated contact that follows.
Mesh contact rather than scratching
Corresponding author Lang Zhou told pv magazine that photoresist printing differs fundamentally from conventional silver paste printing. In silver paste screens, openings account for only 2–5% of the total area, and the remaining surface is covered by an emulsion layer that keeps the mesh from touching the wafer. Full-area photoresist coating, by contrast, typically uses a screen without emulsion coverage so that resist is deposited uniformly across the wafer, which means the mesh comes into direct and extensive contact with the wafer on every printing cycle.
Efficiency drift over 15,000 cycles
Earlier production data pointed to a gradual efficiency decline from 26.2% to 25.7% across 15,000 consecutive printing cycles in commercial cell manufacturing. The loss appeared mainly as lower open-circuit voltage and fill factor, while short-circuit current density and electrical resistance stayed largely unchanged. Minority carrier lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 cycles.
Using three-dimensional confocal microscopy, the team traced the effect to progressive wear of the screen mesh knuckles. As the knuckles flatten, their contact area with the wafer grows, placing greater mechanical stress on the passivation layers beneath. Scanning electron microscopy revealed no visible surface scratches, but photoluminescence measurements confirmed higher recombination losses, pointing to damage at the amorphous silicon/crystalline silicon interface.
A buffer layer and its trade-off
To interrupt that contact, the researchers added an emulsion buffer layer to the screen. They evaluated six patterns with emulsion coverage ratios from 2.9% to 16.6% and found a trade-off: higher coverage protects the wafer but impairs photoresist distribution. A coverage ratio of 4.7% gave the best balance, holding minority carrier lifetime degradation to 0.41% after 10,000 printing cycles while keeping coating uniformity relatively good. The group attributes the improvement to the emulsion layer preventing direct mesh-to-wafer contact and thereby reducing cumulative mechanical damage to the passivation stack.
“The findings demonstrate that a relatively simple modification to screen design can substantially mitigate printing-induced degradation, offering a practical approach to improving the manufacturing reliability of copper-plated HJT solar cells,” Zhou said.
The results were published in Solar Energy as “Screen-printing photoresist induced efficiency degradation and mitigation in Cu-plated SHJ solar cells.”
Copper contacts gain ground
The work comes amid widening interest in replacing silver contacts with copper in HJT cells. In April 2026, researchers at China’s Nankai University reported a silver-free HJT cell at 25.2% efficiency, combining plasma-induced interface engineering with copper electroplating and addressing adhesion, contact resistance and stability at the ITO interface.
Separately, scientists at Germany’s Forschungszentrum Jülich reached 23.08% in a fully copper-metallized HJT cell, a relatively small efficiency penalty against its silver-metallized counterpart, while a configuration using silver-copper paste on the front side and silver contacts on the rear reached 23.95%. Those results underline copper’s potential to reduce silver consumption, although processing and electrical performance still require further improvement.