Rubber & Plastic Products

Natural Pigments Compounded in PLA and PBS, but Heat and Light Limit Performance

Nadia SorensenNovember 2, 20265 min read1 views

At a glance

  • A study of spirulina, curcumin, beetroot and chlorophyllin masterbatches found conventional processing was workable for most formulations, while spirulina failed in PLA and UV stability remained the main gap.
  • Researchers produced natural-pigment masterbatches in PLA and PBS and tested them at 2–6 wt%, finding limited changes in melt flow and mechanical properties for most formulations. Spirulina lost its blue color during PLA processing, and most samples showed perceptible color change after 50 hours of xenon exposure, pointing to light stability as the main barrier.
Four colored polymer strands and natural pigment powders are shown beside PLA and PBS pellets in a conceptual materials-processing scene.

A new study examined whether four commercial natural pigments can be compounded into polylactic acid (PLA) and polybutylene succinate (PBS) without losing color or disrupting conventional melt processing. The pigments were blue spirulina, yellow curcumin, red beetroot and green chlorophyllin. Researchers produced color masterbatches by twin-screw extrusion, diluted them at 2, 4 and 6 wt% in the matching polymer and injection-molded test specimens.

The formulations also contained titanium dioxide, calcium carbonate and stearic acid. The study said these additives were included to support UV protection, dispersion and processing. The work focused on whether natural colorants could withstand industrial conditions while maintaining color, flow behavior and mechanical performance.

Heat narrows the processing window

Thermal stability was the first constraint. Thermogravimetric analysis found degradation onset temperatures of about 229 °C for spirulina, 244 °C for curcumin, 258 °C for chlorophyllin and 267 °C for beetroot. PLA and PBS showed considerably higher degradation temperatures, but their melting requirements still expose pigments to heat.

The researchers therefore used extrusion profiles that melted each polymer while limiting thermal exposure. Processing temperatures reached 145 °C for PBS and 190 °C for PLA. The twin-screw extruder ran at 65 rpm with a feed rate of 2 kg/h.

Most pigment-polymer combinations fit this window, but spirulina was a clear exception. It lost its characteristic blue color during PLA processing, so a blue PLA masterbatch could not be produced. PBS, processed at the lower temperature, retained enough pigment stability for successful compounding. The result shows that pigment compatibility depends strongly on the thermal requirements of the polymer matrix, not only on the pigment's standalone degradation temperature.

Flow and mechanical effects remain modest

From a processing perspective, the natural pigments caused only limited changes in rheology. Melt flow rate fell slightly after incorporation, indicating a modest rise in melt viscosity. Neat PLA had an MFR of about 50 g/10 min, and the natural-pigment masterbatches stayed close to that value. PBS showed a similar response, with only a minor reduction.

For compounders, that result matters: a natural color system offers little practical value if it requires major changes to screw design, pressure settings or molding conditions. In this study, conventional twin-screw compounding and injection molding handled most formulations without major processing problems.

Mechanical properties also remained close to baseline across the 2 to 6 wt% addition range. PLA started with a Young's modulus of about 1710 MPa and tensile strength of 65.6 MPa. PBS started at about 392 MPa and 34.5 MPa. The colored formulations stayed near those values, and impact strength remained in a similar range, although individual pigments produced some variation.

Light stability is the main barrier

Successful extrusion did not guarantee long-term color stability. After 50 hours of xenon-lamp exposure, most formulations showed a color difference above ΔE* = 2, indicating a visually perceptible change. The PLA formulation containing 2 wt% green chlorophyllin masterbatch had the highest photostability and remained the main exception.

The study therefore identifies UV stability as the largest barrier to broader use. Packaging, consumer products, agricultural parts and outdoor applications may need additional stabilization, protective coatings or pigment modification before natural colors can compete with conventional systems over long service periods.

The environmental comparison favored the natural pigments under the study's assumptions. One kilogram of curcumin pigment generated about 0.04 kg CO2-eq, compared with 18.65 kg CO2-eq for the inorganic green reference pigment. The natural-pigment masterbatches also consumed less electricity during extrusion and pelletizing.

The study concluded that several natural colorants can be compounded into PLA and PBS using conventional equipment, with limited changes in melt viscosity and mechanical performance. Further development is still needed, particularly in lightfastness and thermal stability, and future work should focus on color stability during processing and subsequent service exposure.

Reported by Nadia Sorensen, Extrusion, Film and Plastic Packaging Specialist.